Which Aluminium Grade Is Best for Deep Drawing?

Group of deep drawn stainless cups, flanged shells, bosses and retaining rings made by AUNOV

5052 aluminium in the soft O temper is the grade we recommend for a genuine deep draw; 3003 suits shallower, simpler shells; 6061 is not a deep drawing grade at all. The alloy name alone is not a specification — temper, blank diameter and the number of reductions decide whether the part forms or cracks. On our presses 5052 reaches a limiting draw ratio of 1.80–1.95, against 1.85–2.05 for 304 stainless steel and 2.1–2.2 for DC04, so an aluminium shell usually needs one more reduction than the same geometry in deep-drawing steel.

Key point: Pick 5052-O for a seamless deep shell, 3003-O for a shallow cosmetic cover, and keep 6061 for shallow forming followed by heat treatment — never for a multi-stage draw.

The grade decision in one table

Material selection for deep drawing is a formability decision first and a strength decision second. The forming limit of a sheet is described by its limiting draw ratio (LDR), the largest blank-diameter to punch-diameter ratio a single draw survives without tearing; the underlying r-value and n-value test methods are standardised as ASTM E517 and ASTM E646. ASM Handbook Volume 14B covers how those properties translate into a draw schedule. The figures below are the values we quote from our own press data, not generic handbook numbers.

What matters in practice is the reduction per stage. A 5052 blank with an LDR of 1.80–1.95 cannot take the same first reduction as a DC04 blank at 2.1–2.2. The limiting draw ratio chart shows those bands side by side; the drawing calculator turns them into a stage estimate before any tool is cut.

Why 6061 behaves differently

6061 is a heat-treatable Al-Mg-Si alloy. In T6 condition it has already been solution treated and artificially aged, so it has high yield strength and little remaining ductility: it cracks on a deep draw. In the annealed O temper it can be formed, but it still work-hardens faster than 5052 and loses the seamless-wall consistency a filter housing or battery can needs. Our position is documented in Can 6061 Aluminium Be Deep Drawn?: we do not deep draw 6xxx sheet. Where the print calls for final T6 strength, we form shallow and heat treat afterwards, and we state the distortion and tolerance consequences up front.

5052 aluminium alloy is a non-heat-treatable Al-Mg grade whose strength comes from solid-solution and cold work, which is why it stays formable through successive reductions. For a deeper comparison across steel, stainless steel and aluminium, see material selection for deep drawing.

What the drawing should say

Specify the alloy, the temper and the functional tolerance together. A drawing that says only “aluminium” leaves the blank diameter, the anneal state and the inspection band undefined. Our formed dimensions are held to ±0.05 mm as standard, tightening to ±0.02 mm on features that receive an ironing pass. We run 5–500 ton presses, draw to 150 mm depth, build the tooling in-house and return a quote within 24 hours; minimum order quantity is 1,000 pieces per part number. Quality records follow ISO 9001.

If the part is not round, the corner radius rather than the grade becomes the first constraint — see irregular deep drawn parts. For a worked example of a seamless aluminium shell in production, see the oil and fuel filter housing guide.

Decision table

aluminium grade forming route why
A seamless can with real depth 5052-O Highest LDR of the common Al-Mg grades we draw (1.80-1.95)
A shallow cosmetic cover 3003-O Easy to form, good surface after a single reduction
T6 strength on the final print Shallow form 6061, then heat treat 6061-T6 cracks on a multi-stage draw
Tight bore tolerance 5052 plus an ironing pass Ironing tightens the formed wall to +/-0.02 mm
Any grade, non-round footprint Review corner radius first Material flow differs at every angle

Frequently asked questions

Can 3003 aluminium be drawn as deeply as 5052?

3003 forms easily but does not hold the same wall consistency through repeated reductions as 5052. For a shallow cover it is the more economical choice; for a tall seamless can we quote 5052-O. The stage plan is set by the limiting draw ratio, and we confirm it per drawing rather than publishing a single universal depth.

Does the O temper change what 5052 can do?

Yes. O temper is the soft, annealed condition and gives the alloy its full formability. A harder temper raises yield strength but consumes ductility, so the same geometry needs more reductions or an intermediate anneal. Always state the temper next to the grade on the drawing.

At which forming stage does 6061-T6 fail on a multi-stage shell?

T6 is a solution-treated and artificially aged condition: strong, but with too little ductility left for the plastic flow a deep draw demands. It tears at the punch radius. Even in O temper it is a poor choice for a multi-stage shell compared with 5052.

Which aluminium grade holds the tightest wall tolerance after ironing?

The grade matters less than the operation. Our formed dimensions hold +/-0.05 mm, and an ironing pass brings the wall and bore to +/-0.02 mm. That figure is an ironing result, not a property of 5052 or 3003 alone.

Do aluminium shells need a different blank holder setting than steel?

They do. Aluminium has a lower forming limit and different friction against the die, so blank holder force, die radius and lubrication are set from the grade rather than copied from a steel job. The limiting draw ratio is the starting point for that decision.

Besides grade and temper, which five fields belong on a deep drawing print?

Alloy, temper, blank or finished diameter, depth, the dimensions that carry a functional tolerance and the surface requirement. With those five items we can return a stage plan and a quote within 24 hours. See the Engineering Guides hub for the design checks behind each one.

What we do not claim: We do not publish leak-rate figures, autoclave cycle counts, springback angles or furnace recipes that we have not measured on our own parts. The ±0.02 mm figure applies to ironing passes only, not to every geometry. 6xxx aluminium is used for shallow forming, not deep drawing. Prices, minimum order quantities and lead times are confirmed per drawing rather than published as fixed values.

Last reviewed: 2026-11-05 · Reviewed by Sam Zhang, Process Engineer. See the full Deep Drawing Engineering Guides hub for process comparisons, measured draw ratios and defect troubleshooting.