Polished CNC Turned Cross Fitting

Specifications

Frequently Asked Questions

Why is the branch hard in two independent ways?

Direct answer: Because the branch is a geometric interruption and a stress concentration at once. The hole breaks the wall, and the transition from the main body to the branch is where the stress concentrates. The two are independent: a branch can be geometrically clean and still be a stress riser.

Polishing this branched part is hard at one place – where?

Direct answer: Because the branch and the body meet at a radius, and polishing that junction without wiping out the geometry is hard. The polish has to follow the surface into the corner, and the corner is where the finish matters most and is hardest to reach. The polish is a geometry-preserving operation, not just a surface one.

Why does this part list both aluminium and steel?

Direct answer: Because the two halves of the duty pull different ways. One end may want aluminium’s lightness or conductivity, and the other wants steel’s strength or wear. The part is specified in both because a single material cannot serve both ends, and the choice is made per feature.

ItemAluminum and Steel CNC Turned Caps and Fittings
BrandAUNOV
DesigningMade to your 2D/3D drawings (PDF, DWG, STEP, IGS) – samples are reverse-measured into a controlled drawing; revisions are re-quoted once rather than silently absorbed.
ToolingOur toolroom covers die design, wire-cut EDM and maintenance, so die cost stays transparent, and first-article timing is measured from the tooling start date.
SamplesSamples are issued for approval before the run, so any deviation is corrected at sample stage, and later batches are gauged back to the signed sample.
MaterialsStock runs to carbon steel, 304 / 316 stainless steel, aluminium and brass; material substitutes are proposed only with your written approval.
Surface finishZinc, nickel or chrome plating, anodising, passivation or e-coat; finish thickness and adhesion checked on the first article.
ProcessingTurning, milling and drilling sequenced to minimise handling and re-chucking; batch records are filed so a repeat order starts from approved data.
EquipmentTurning centres fed from bar, with machining centres for milled features, backed by CNC turning centres and a climate-controlled inspection room.
Tolerance+/-0.02 mm general machining, tighter on flagged dimensions; dimensional reports accompany the first article.
Delivery termsFOB Ningbo or Shanghai, T/T with deposit and L/C for larger runs; each volume tier carries its own quoted price.

A polished cross fitting is a fluid fitting with four branches at right angles, and the right angle is the whole design problem. Fluid fittings fail at the branch for two reasons that have almost nothing to do with each other: the branch is where the flow changes direction and the pressure disturbance is highest, and the branch is where the two features that have to meet – the tapped port and the run of the main body – have to physically coexist in a limited amount of metal.

Add polishing to it and you get a third requirement that interacts with both: a polished surface has no place for a burr, and a burr in a fluid passage is a contaminant and a turbulence generator.

Why the branch is hard, in two independent ways

The flow problem

At a ninety-degree branch the flow separates. The separated region creates turbulence and, more importantly in a liquid service, cavitation – local pressures fall below the fluid’s vapour pressure in the corner downstream of the branch, and vapour bubbles form and collapse. The damage that results is pitting at exactly the branch point, and it is progressive because the pitting becomes the nucleation site for the next generation.

Three design responses, all of them geometric:

  • A radius at the intersection. A sharp internal corner is where cavitation initiates. A generous radius at the branch removes the sharp corner and it is the single most effective change available. On a cross fitting, this is the difference between a part that lasts and a part that pits.
  • Branch bore size relative to the main bore. A branch that is nearly as large as the main flow is easier to make and, on a fitting, more likely to be what the flow needs. A very small branch fed from a large main creates a high-velocity jet into a low-pressure region, which is the worst combination for cavitation.
  • The angle. A true ninety degrees is the worst case for flow separation. Where the design allows it, a pair of forty-five degree elbows is dramatically better – and on a turned part that means either two parts or a much more complex geometry.

The manufacturing problem

On the manufacturing side the branch is hard for a structural reason: the branch is a hole drilled radially into the main body, and where it breaks through, it removes the main bore’s wall at the top and bottom. The metal between the branch’s outer edge and the main body’s outer edge is a thin section that has to carry the joint’s load and survive the machining.

Three practical consequences:

  • The branch’s breakthrough weakens the main bore locally. On a part carrying pressure, the remaining ligament between the branch and the outside of the body is a stress concentration and it is where a pressure fitting fails. The wall thickness there is a real design dimension.
  • The drilled branch’s exit into the main bore leaves a burr or a sharp lip, and that lip is exactly where the flow separates. A burr there is both a contaminant and a nucleation site for cavitation. Deburring the intersection – internally, at the point where two holes meet – is one of the harder operations on a machined fitting and it is frequently skipped.
  • Threading after drilling matters. On a cross fitting the branch will usually be tapped after the main bore and the branch are drilled, and tapping into a drilled hole produces a burr at the thread’s mouth that sits directly in the flow.

Polishing, and why it is harder than it sounds on this part

Polished, per the print, with the agreed finish travelling with the part number. On a fluid fitting “polished” is one word covering four quite different surface conditions, and the distinction matters because they behave differently in flow.

  • Electropolishing. A cleaner process that produces a smooth, thin oxide-free surface. It is the right process for stainless steel in a fluid service and it does not smear the metal, which is the main risk on stainless steel.
  • Mechanical polishing with abrasive, on a lathe. Produces a bright surface on the external and the accessible internal surfaces. The risk is that it smears the metal – it pulls a layer of soft metal across the surface and it can partly close a hole. On a fitting’s small bore, mechanical polishing can reduce the diameter measurably and it will leave a smeared surface that sheds particles.
  • Passivation after polishing. On stainless steel this is not optional if the part is in a corrosive service, because polishing removes the passive layer and passivation restores it.
  • Blasting or tumbling for a uniform matte or satin appearance, which is a different thing again and is chosen for handling rather than for flow.

So on a polished cross fitting the specification needs to say: which process, on which surfaces – internal or external or both, and if internal, how deep – and whether the dimensions are before or after polishing. And for the internal surfaces, a roughness value with a convention, because a polished internal surface that is not specified will be polished externally and only nominally finished inside.

Material, and why this part lists both aluminium and steel

Carbon steel, 304 and 316 stainless steel, aluminium and brass, with substitutions proposed only in writing. On a fluid fitting the material is chosen by the fluid and the pressure, and there are four specific notes.

  • Brass is the traditional fluid fitting material and it is the right answer for most water and fuel and general instrumentation service. It is easy to machine to a fine finish and it polishes well, and its corrosion behaviour is good except in dezincification-prone environments.
  • Stainless Steel 316L for chloride-bearing or aggressive service and for any welded condition. Stainless Steel is harder to machine, harder to polish without smearing, and it will work-harden – so on a cross fitting the branch’s drilling should be continuous and the finish process should be electropolish rather than abrasive.
  • Aluminium is used on this route for light or low-pressure applications, but it is a poor choice for a fluid fitting’s general use for two reasons: it galls against steel fittings and fasteners in a way that will seize a joint, and its fatigue strength is low, which matters on a part that is repeatedly assembled.
  • Carbon steel where the fluid is benign and the pressure is moderate, with a plating or coating because bare steel in a wet fluid fitting will rust internally and the rust will contaminate the fluid and the passage.

Tolerance, allocated to the seal and the thread

+/-0.02 mm general machining with tighter bands on the flagged dimensions, dimensional reports accompanying the first article. On a cross fitting the flagged dimensions are the sealing and threading features, and they are concentrated at the ports.

  • Thread class and pitch diameter on every port, gauged. The cross fitting is distinguished from a single fitting by having four of them, and each one is a potential leak path, so each one is a separate inspection item rather than a general requirement.
  • Port face flatness and perpendicularity to each port’s axis, where the seal is a face seal or a bonded washer. A port face that is not square to its axis will not seal evenly, and on a cross fitting this is easy to miss because there are four faces and they are all machined in different directions.
  • Seat or chamfer geometry on each port, which is functional on a taper-sealing port and is not merely a lead-in.
  • Concentricity of each port’s axis to the fitting’s main axis, and their angular relationship to each other. Two ports that are 89 degrees apart instead of 90 is a real assembly problem.
  • The main bore’s diameter and its internal finish, and the branch bores’ diameters, stated pre- or post-polish.
  • External dimensions at a general band.

Inspection, in the order that matters on a four-port part

  1. Every port thread gauged, every port on every part. This is the item that scales with the number of ports and it is the one most often sampled rather than checked.
  2. A functional pressure or leak test on every port of every part. On a fluid fitting this is the only test that tests the specification, and on a four-port part it is four tests. This is the single highest-value inspection item on this page.
  3. Internal bore sizes and finish measured after polishing, with the measurement method stated, because polishing changes them.
  4. The branch-to-main-bore intersection, inspected for burrs and for the internal radius. This is a visual and tactile inspection and it needs an agreed standard because it is a subjective item and it is the most important internal feature on the part.
  5. Port face flatness and perpendicularity on the face-sealing ports.
  6. CMM data on the port positions relative to the main axis, and the angular relationships.
  7. Surface finish on the polished surfaces, on the first article, with the internal surfaces explicitly included in the scope.
  8. Passivation recorded on stainless steel, where it is specified, because it is what makes the polished part corrosion-resistant again.

Liquid or gas, at what pressure, in which direction

Is this fitting carrying liquid or gas, and at what pressure – and is the flow direction known? Those three answers decide most of the design on this part. Liquid at pressure means cavitation is a real risk and the branch’s internal radius becomes a life-determining dimension, and the flow direction tells you which branch sees the separation and which does not, so in a symmetrical cross fitting the two branches may need different radii even though they look identical. Gas means cavitation is much less of a concern and the pressure drop through the small branch becomes the limiting factor instead, which changes the sizing entirely. And the pressure decides whether the branch’s breakthrough ligament is a structural calculation or whether the fitting is simply a fitting. It is worth noting that most cross fittings are specified by nominal size and thread and pressure rating and by nothing else, and that on a part with four branches the absence of a flow direction is the absence of the information that would let the internal geometry be optimised. Naming the flow direction on the drawing costs one arrow.

Request a Quote for This Part

Send a drawing or sketch — get material advice, tooling cost and a per-piece price within 24 hours (working days).