Deep Drawn Tubes & Cans: How Seamless Metal Parts Get Made
A deep drawn tube is a hollow, seamless metal part shaped by pushing a flat sheet blank through a series of ring-shaped dies in a single, continuous press stroke. The metal flows and thins instead of being cut away, so the finished part carries no weld seam and gives fluid or gas nowhere to leak. That one property — seamless — is the reason battery cans, sensor housings, and filter shells get drawn rather than spun, turned, or welded together.
At AUNOV we draw tubes, cans, shells, and enclosures from stainless steel, aluminum, and copper on presses running from 5 to 500 tonnes. Wall thicknesses land between 0.15 and 3.0 mm. We hold ±0.05 mm as a baseline tolerance, and ±0.02 mm on diameters once an ironing pass is added. Drawing depth reaches 150 mm. Those figures are what buyers actually quote against, so I will keep returning to them as we go.
What deep drawing actually does to the metal
Picture a flat disc of sheet. The press clamps its outer edge and drives a punch straight down into a die cavity. The disc does not get punched out — it gets squeezed and stretched into a cup. Each successive station has a slightly smaller diameter and (often) a tighter punch-to-die gap, so the cup grows taller and the wall gets thinner and more uniform. By the last station you have a tube, a can, or a deep shell with walls measured in fractions of a millimetre.
The word “deep” is not marketing. It describes the ratio of draw depth to starting diameter. Once that ratio passes roughly 0.5, you are no longer stamping a shallow lid — you are deep drawing, and the metal behaviour changes. It work-hardens. It wants to wrinkle at the flange or tear at the base. Controlling those two failure modes is most of the craft.
Why a seamless tube beats a welded one
Welds are weak points. They are also leak paths waiting to happen, and they interrupt the grain flow of the metal so corrosion finds a seam to start in. For a battery can holding electrolyte, a fuel line fitting, or a pressure sensor body, a single uninterrupted wall removes an entire class of failure.
Seamless also means consistent wall thickness around the full circumference. A rolled-and-welded tube always carries a slight thickness step at the seam. A drawn one does not. When your spec says ±0.05 mm, that consistency is what lets the rest of the assembly fit.
There is a second, quieter benefit. Because deep drawing is a cold-forming process, the part leaves the press near net shape. You machine little or nothing afterwards. That cuts both scrap and cycle time, which is how a part that looks complex ends up cheaper than you expected at volume.
Which metals we draw into tubes and cans
Stainless steel is the workhorse. Grades in the 300 series — 304 above all — draw cleanly and resist corrosion without coating, which is why so many sensor and medical parts are made from it. We also run 400-series and duplex grades when hardness or magnetism matters.
Aluminum draws beautifully and keeps weight down. The 3000 and 5000 series (5052 in particular) are common for enclosures and battery components where mass matters more than ultimate strength. Copper and its alloys turn up where conductivity or brazing behaviour drives the design — capacitor cans are a good example.
Material choice sets your limiting draw ratio, and that number decides how deep a part you can make before the wall tears. As a rule of thumb from our own presses: low-carbon steel such as DC04 reaches a draw ratio around 2.1 to 2.2, 304 stainless steel about 1.85 to 2.05, and 5052 aluminum roughly 1.80 to 1.95. Push past those and you are asking the metal to do something it physically will not.
How the process actually runs, station by station
It starts with a blank. We shear or laser-cut a disc to a diameter calculated from the final part volume, because the metal has to go somewhere and over-blanking just wastes material.
First draw forms the initial cup. Second and later draws narrow it and pull it deeper. If the spec calls for a tight diameter tolerance, we add an ironing pass where the punch and die squeeze the wall to a precise, even thickness — that is where the ±0.02 mm figure comes from. Trimming cuts the top edge square. Then come the secondary operations: threading, notching, piercing holes, coining a flange, or knurling. We do these in-line so the part ships finished rather than as a rough shell you have to sort out elsewhere.
Tooling is the part people underestimate. A multi-station progressive die is not something you buy off a shelf. We design and build our tools in-house, which means the draw schedule, the radii, and the ironing gaps are tuned to your specific alloy and geometry instead of to a generic compromise. It also means when a dimension drifts, we fix the die ourselves in hours, not weeks.
Tolerances, wall thickness, and what is realistic
Wall thickness is the first question every buyer asks and the hardest to answer in one number, because it depends on the alloy and the depth. Our working range is 0.15 to 3.0 mm. Below that you fight springback and tearing; above it you are usually better off with a different process.
Diameter and length hold ±0.05 mm as a standard, tightening to ±0.02 mm on ironed diameters. Concentricity between the tube axis and a feature such as a threaded neck is where drawn parts shine, because everything is referenced to the same die centreline.
One thing worth saying plainly: depth and thin wall fight each other. A 150 mm deep part at 0.15 mm wall is at the edge of what cold drawing will give you reliably. If your design needs both, talk to us early — often a small change in the neck or a two-piece assembly opens up a process that simply will not work as a single draw.
Where you already see deep drawn tubes and cans
Walk through any modern device and you will find them. Cylindrical battery cans — the steel or aluminum shells in cells — are deep drawn by the billion. Sensor housings for temperature, pressure, and position sit in stainless steel shells drawn to seal against harsh media. Filter shells, capacitor cans, and the little enclosures that hold electronics in cars and industrial gear are all the same family of part.
The through-line is always the same: a closed, sealed, sometimes pressurised volume made from one piece of metal. When the cost of a leak is a recalled product, seamless wins.
Designing a part that draws well
If you are at the drawing board, a few habits save money. Keep wall thickness even around the part — steps and sudden thin sections are where tearing starts. Give the base a generous radius rather than a sharp corner; the metal needs somewhere to flow. Spec tight tolerances only where they matter, because every extra tenth of a millimetre costs you in tooling and scrap.
Think about the opener, too. A part that needs a precise internal shoulder for a weld or a crimp is straightforward to draw; one that needs a complex internal thread is better served by adding that operation after the shell exists. We are happy to look at a sketch and tell you which features belong in the draw and which belong downstream.
Why buyers come to AUNOV for this
We are not a job shop that happens to own a press. Deep drawing is the core of what we do, and the numbers reflect that focus: 5 to 500 tonne presses, walls from 0.15 to 3.0 mm, ±0.05 mm as standard and ±0.02 mm ironed, 150 mm of draw depth, tooling built and maintained in our own shop. We quote within 24 hours and our minimum order starts at 1,000 pieces, which keeps prototyping and first production runs affordable.
More than the spec sheet, the value is in the iteration. Because we own the tooling, a design change does not mean a new vendor and a new lead time — it means a conversation and a revised die. For teams bringing a sealed metal part to market, that loop is usually the difference between shipping and stalling.
Tube depth is what sets the stage count here. The LDR reference works the ratio through stage by stage, and the deep drawing process covers the anneals that sit between those stages.
Frequently asked questions
What is deep drawing?
Deep drawing is a cold-forming process that turns a flat sheet-metal blank into a hollow, seamless part by forcing it through a series of dies with a punch. The metal stretches and thins into a cup, tube, or shell rather than being cut or welded, which leaves the finished part with no seam.
Why choose a seamless tube over a welded one?
A seamless tube has no weld line to leak, corrode, or weaken, and its wall thickness stays even all the way around. For parts that hold fluid, gas, or pressure — battery cans, sensor bodies, filter shells — removing the seam removes an entire class of failure.
Which metals can be deep drawn into tubes and cans?
Stainless steel, aluminum, and copper are the common choices. Stainless steel such as 304 resists corrosion without coating, aluminum such as 5052 keeps weight down, and copper suits conductive parts like capacitor cans. Each alloy has its own limiting draw ratio that sets how deep a part can go.
What wall thickness is possible with deep drawing?
The practical range we hold is 0.15 to 3.0 mm. Thinner walls risk tearing and springback; thicker ones usually suit a different process. Depth and thin wall pull against each other, so a very deep part at 0.15 mm is near the reliable limit of cold drawing.
How tight can deep drawn tube tolerances get?
Diameter and length hold ±0.05 mm as a standard, tightening to ±0.02 mm on diameters that receive an ironing pass. Because every feature references the same die centreline, concentricity between the tube body and a neck or flange is typically excellent. The standard band and the ironing figure are defined on the capacity page, the canonical tolerance reference.
What are the most common deep drawn tube and can applications?
Battery cans, sensor housings, filter shells, capacitor cans, and precision electronics enclosures make up most of the volume. The shared requirement is a sealed, often pressurised volume made from one piece of metal with no leak path.
How do I design a part for deep drawing?
Keep wall thickness even, give the base a generous radius instead of a sharp corner, and apply tight tolerances only where the function demands them. Features like internal threads are usually better added after the shell is drawn. Sending a sketch early lets us flag which details belong in the draw and which belong downstream.
What is the minimum order quantity at AUNOV?
Our minimum order starts at 1,000 pieces, and we return a quote within 24 hours. Tooling is designed and built in-house, so prototype and first-run volumes stay affordable and design changes can be turned around quickly. The volume threshold for new tooling is stated once on the capacity page.
At what gauge does a drawn tube flange start to wrinkle?
We draw tube walls down to 0.15 mm, but the practical floor is set by the flange rather than the wall. Thin blanks buckle before they feed, so we raise blank-holder force, add a draw bead, or step the gauge up. The finished wall is measured on the first article, never assumed from the incoming sheet. The deep drawing reference article sets out the mechanics behind that flow.
Key point: A drawn tube has no longitudinal weld, which is why it is used wherever a leak path is unacceptable.
What we do not claim: We do not publish leak-rate figures, autoclave cycle counts or springback angles that we have not measured. The ±0.02 mm figure applies to ironing passes only, not to every geometry. 6xxx aluminium is used for shallow forming, not deep drawing. Prices, minimum order quantities and lead times are confirmed per drawing rather than published as fixed values.
Last reviewed: 2026-11-05 · Reviewed by Sam Zhang, Process Engineer
Decision path for a seamless tube or can
| If you need to decide | Start here |
|---|---|
| Whether a seamless shell beats a welded one | Drawn vs machined vs welded housings |
| Whether to redraw or to iron the wall | Ironing vs redraw |
| The numeric tolerance bands | Deep drawing capacity |
| The minimum order quantity and quote turnaround | Deep drawing capacity |
| Why 6xxx aluminium is not used for a deep draw | Can 6061 aluminium be deep drawn? |