A shallow pan’s only hard requirement is flatness, and it is the one most often missed
A shallow drawn rectangular pan is a shallow rectangular dish with a flange. It is one of the least demanding shapes in this family to form, and one of the easiest to get subtly wrong, because almost all of its value is in a property that a dimension report does not capture: flatness. A shallow pan is a plate, a plate is only as good as its flatness, and a drawn plate is not flat – it is dished, bowed, or twisted, and how much depends on the geometry, the material, and what happens to the part after it leaves the tool.
We deep draw from coil or blank with in-process annealing so walls thin evenly, with in-process checks between stages, on mechanical presses from 5 to 250 T and hydraulic presses 250-500 T with in-line annealing furnaces, with CNC turning centres for secondary operations and CMM inspection. Formed features to +/-0.05 mm with capability data on critical dimensions, and GD&T per the drawing with PPAP-style reports on request. Stock runs to carbon steel in SPCC and DC01 grades, 304 and 316 stainless steel, aluminium and brass, with mill certificates and heat numbers accompanying the first article. Finish is selected from the drawing – plating, coating, anodising or passivation – with the finish inspected alongside the dimensional report on the first article. This page is about flatness: why it is the requirement, what causes it, and how it is specified and controlled.
Why a drawn pan is not flat
Forming a pan’s walls from a flat blank leaves the pan’s base with residual stress, and residual stress moves. Four causes, and they are all present on a typical pan:
- Forming stress. Drawing the walls stretches the material around the base’s perimeter and leaves the base in a state of tension or compression. That stress relaxes over time and over handling, and as it relaxes the base moves.
- The corner effect. On a rectangular pan, the corners are the most stretched part of the whole blank. Four corners pulling in four directions against a base that is not itself drawn produces a base that is not flat, and – crucially – the corners are not symmetric, so the pan is often twisted rather than merely dished. A twisted pan is worse than a dished one because it will rock on a surface.
- Wall thickness variation. The base is supported by the die during drawing and is the strongest part of the pan, while the wall is thinned. Where the base and the wall meet, the transition is a stiffness discontinuity, and it is where bending concentrates. A base whose thickness varies around its perimeter is a base that will dish.
- Handling and stacking. This is the cause that appears long after manufacturing. A shallow pan is easy to bend, pans are stacked, and a pan that has been under a load in a box will not be flat on arrival. No manufacturing control fixes this.
Where the pan’s flatness actually matters
Three functional reasons, in descending order of how often they matter:
- It seats on something. A pan that locates in a frame, nests in a rack, or sits against a mating surface needs to be flat, and a pan that is not flat will either rock or sit with a gap at one corner. This is the most common reason and it is a straightforward positional requirement.
- It seals. Where the pan’s flange seals against a cover or a lid, the flange’s flatness is the seal’s flatness, and a dished flange leaks at its high point. This is the same requirement as on any enclosure, and it is a functional tolerance rather than a preference.
- It carries a load in a supported way. A pan used as a base for something – a plate that stacks items, a tray that carries product – needs to distribute that load. A dished pan concentrates it on the high point, and anything sitting in it will rock.
Forming features that make a pan stiff
The most effective way to make a shallow pan flat is to give its base some stiffness, and there are three ways to do it – and the choice is a genuine trade against cleanability and material use:
- A formed rib or bead across the base. The cheapest and the most effective. A rib raises the base’s moment of inertia substantially for very little material, and it is a single forming operation. The trade is that a rib is a feature on a surface that may need to be cleanable, and a rib that forms a pocket will hold residue.
- A rolled or drawn edge around the base’s perimeter. A hem or a return flange around the base stiffens it and also protects the edge. It costs material and it makes the pan deeper.
- A thicker base. The expensive answer. It works and it uses more material for the same stiffness, and on a shallow pan the material is a meaningful fraction of the part’s cost.
Materials, and their effect on flatness
Stock runs to carbon steel in SPCC and DC01 grades, 304 and 316 stainless steel, aluminium and brass, with mill certificates and heat numbers accompanying the first article. On a pan where flatness is the requirement:
- DC01 over SPCC where the incoming material’s variation matters. DC01 has tighter mechanical property tolerances, and on a part where residual stress drives the flatness, a consistent material gives a consistent result. This is a real and inexpensive improvement on a part whose only hard requirement is flatness.
- Aluminium is the most formable of the group and produces the least springback, so it is the best material for a flat pan. It is also the most prone to dishing under a point load and it deforms more easily in handling, so the handling requirement matters more rather than less.
- 304 or 316 stainless steel springs back substantially more than mild steel, and a drawn pan in stainless steel will have a different and slightly more variable flatness than the same pan in steel. Stainless Steel also work-hardens at the corners, which stiffens the corners and makes a twisted distortion more likely rather than less.
- Carbon steel with plating gives a stable, low-cost pan with good flatness, and the plating is what provides the surface. Where the pan is visible, the plating’s uniformity is a visual requirement.
Specifying flatness properly
Formed features to +/-0.05 mm is the dimensional band, and flatness is a separate callout with its own requirements. Four things a flatness specification has to state to be measurable:
- What surface it is measured against. The pan’s base measured to a surface plate, or the pan’s flange measured on its own plane, or the pan seated on a surface. These give three different numbers for the same part.
- How the part is supported during measurement. A pan measured on three points is being measured for twist as much as for flatness, and a pan measured unsupported is being measured for something else. Where the requirement is about how the part sits in service, the measurement should reproduce how it sits in service.
- Total flatness versus local flatness. A pan can be within a total flatness band and still have a local high spot in the middle. Where something sits in the pan, local flatness is the requirement; where it seats on a surface, total is.
- The measurement condition, including temperature. A thin pan changes dimension with temperature, and measuring a pan warm and using it cold puts a real error into the number.
Finishing, and the two surfaces that must be treated differently
Finish is selected from the drawing – plating, coating, anodising or passivation – with the finish inspected alongside the dimensional report on the first article. On a pan:
- Mask the sealing flange where the pan seals against a cover. A coating there changes the seal’s geometry and its compression.
- Coating adds thickness on both faces, which slightly increases the pan’s depth and its flange’s thickness. On a pan with a general dimensional band this is not significant; on a pan with a fitted depth it is, and the drawing should say.
- Coating the base stiffens it. A thin coating adds a small amount of material to a surface and increases its stiffness very slightly – which is occasionally a useful side effect and is not a substitute for a rib.
- Where the pan is visible, the base’s surface is the product, and a drawn base carries draw marks and the coating’s own texture. A retained colour and gloss reference sample is worth more than a finish code on a visible pan.
A shallow pan needs no tooling to form
Seven things, and the first is the one that is usually missing:
- Flatness, with the surface it is measured against and the support condition. Total or local, and the surface named.
- Whether the pan must seat, seal, or carry a distributed load, because each of those implies a different flatness requirement and a different measurement.
- Flange flatness and parallelism against a named surface, separately from the base, if the flange seals.
- Any rib or stiffening feature, with its geometry and the direction it drains, if the base is cleaned.
- Wall thickness and base thickness, and whether the base is thicker than the wall – which is common and worth stating, because a pan with a uniform thickness is a pan with a dishable base.
- Material grade, and DC01 over SPCC where flatness is the governing requirement.
- Which surfaces are masked, and whether dimensions apply before or after finish.
Does this pan need to be drawn at all?
Does this pan need to be drawn at all? A shallow pan is a formable shape in almost any material, and the alternatives are a machined or folded pan. A folded pan from sheet – cut, bent, and welded or brazed at one corner – is very cheap at low volume and gives a much flatter result than a draw, because there is no drawing stress. A drawn pan wins on volume, on a seamless one-piece construction, and on material efficiency. The trade is exactly flatness against cost: a folded pan is flatter, a drawn pan is cheaper at volume. For a pan whose only requirement is that it be flat and hold something, a folded or machined pan is frequently the better answer, and it is worth asking at enquiry which side of that trade the product wants.
Choosing between drawing, machining and welding comes down to the shape of the part: the guide to deep drawn covers sets out where each route wins, and the overview page links through to the full Precision Deep Drawn Parts range.
Specifications
| Item | Stainless Steel Shallow Drawn Rectangular Pan |
|---|---|
| Brand | AUNOV |
| Designing | Send drawings, or send a sample to be measured – samples are reverse-measured into a controlled drawing; revisions are re-quoted once rather than silently absorbed. |
| Tooling | Tooling is built and held under your part number, so a die can be re-cut against the approved drawing, and first-article timing is measured from the tooling start date. |
| Samples | Samples are issued for approval before the run, and production starts only after written sign-off. |
| Materials | Stock runs to carbon steel, 304 / 316 stainless steel, aluminium and brass; mill certificates and heat numbers accompany the first article. |
| Surface finish | Finish selected from the drawing: plating, coating, anodising or passivation; the finish is inspected with the dimensional report on the first article. |
| Processing | Deep drawing from coil or blank, with in-process annealing so walls thin evenly; in-process checks sit between stages, not only at the end. |
| Equipment | 5-250 T mechanical presses, 250-500 T hydraulic presses and annealing furnaces in line, backed by CNC turning centres and a climate-controlled inspection room. |
| Tolerance | +/-0.05 mm on formed features, with capability data on critical dimensions; GD&T per drawing, PPAP-style reports on request. |
| Delivery terms | FOB Ningbo or Shanghai, payment by T/T or L/C, quoted in USD or EUR; repeat orders reuse the approved first article. |
Frequently Asked Questions
Why is flatness the key requirement of a shallow drawn pan?
A shallow pan is a plate, and its value is flatness. A drawn plate is dished, bowed or twisted depending on geometry, material and post-tool handling, so flatness is specified and controlled, never assumed from the dimension report.
How is flatness controlled on a drawn stainless steel pan?
Drawn features are held to +/-0.05 mm with capability data on critical dimensions and GD&T per the drawing. The flange flatness is checked and reported on the first article so the seating surface is documented.
Which stainless steel grade is used for a shallow pan?
304 or 316 stainless steel, with mill certificate and heat number on the first article; 316 is used where the duty needs the extra corrosion resistance. The grade is confirmed before tooling.
Can a shallow pan be formed without dedicated tooling?
For moderate volumes a soft tool or an existing family die can form it, and we confirm tooling against the drawing before quoting. The typical minimum order is 1,000 pieces with a 24-hour quotation.
Related Products
Request a Quote for This Part
Send a drawing or sketch — get material advice, tooling cost and a per-piece price within 24 hours (working days).