2026-09-27 09:03:11 larryzhang

SS304 and SS316 are the two austenitic stainless steels most often drawn into sensor housings. By composition, 304 is roughly 18% chromium and 8% nickel (the classic ‘18/8’ grade), while 316 keeps a similar chromium-nickel base but adds 2–3% molybdenum for chloride resistance. When we quote a new deep drawn sensor housing, the most common technical question from customers is also the most practical one: should this part be SS304 or SS316? The two grades look identical, machine almost identically, and cost-wise they are close — but choosing wrong can show up two years later as a warranty claim.

Here is how we guide customers through that decision, based on fifteen years of drawing these exact parts. This guide stays narrow — 304 versus 316 on a sensor housing. For the wider question of which material family to draw in the first place, our material selection guide sets stainless steel against aluminium, brass, copper and steel.

The short answer

Choose SS304 for standard environments; upgrade to SS316 when chlorides are present. If the housing will see road salt, marine air, cleaning chemicals or process fluids, 316 earns its premium. For indoor electronics, appliances and most automotive cabin sensors, 304 does the job at a better price.

What actually separates the two grades

The difference is molybdenum. SS316 contains 2–3% Mo, which dramatically improves resistance to pitting and crevice corrosion — the two failure modes that matter most for a drawn shell, because the drawing process creates exactly the kind of recessed geometry where chlorides collect.

PropertySS304SS316
Corrosion resistance (general)Very goodExcellent
Chloride / salt resistanceLimitedExcellent
Deep drawabilityExcellentVery good
Cost (relative)Baseline+10–20% material
Typical finish after drawingBright, cleanBright, clean

One nuance from the factory floor: 304 draws slightly better. The Mo addition in 316 raises work-hardening rate a little, so for shells with deep draws or thin walls, 304 is more forgiving on die design and press settings. When a customer’s environment doesn’t demand 316, we say so — it saves material cost and can improve dimensional consistency.

Application-by-application guidance

Automotive underbody & wheel-well sensors → SS316. Constant salt spray exposure is the harshest routine environment a sensor housing faces.

Engine bay temperature sensors → SS304 is usually sufficient; 316 for direct exhaust-proximity parts.

HVAC & refrigeration → SS304 for indoor units; SS316 where condensate with treatment chemicals contacts the shell — a common cause of pitting on economizer and expansion valve assemblies. See our deep drawn valve tubes.

Marine, coastal & food-processing equipment → SS316, no debate. Chloride attack on 304 housings in these settings is not a risk, it’s a schedule.

Consumer & office electronics → SS304. Indoor, low-humidity environments never stress the grade.

Why the drawing process matters in this choice

A sensor housing is not a flat coupon. Deep drawing work-hardens the material and concentrates deformation at the punch radius — the same regions where residual stresses are highest. In chloride environments, stressed 304 pits faster than unstressed 304. This is why we see real-world failures on 304 housings that “passed the datasheet,” and why we push 316 more aggressively for drawn shells than a materials chart alone would suggest.

Passivation after drawing helps both grades by removing free iron picked up from tooling. For harsh-duty 304 parts, we recommend it as standard; ask us about surface options.

Bottom line for buyers

Your environmentOur recommendation
Indoor, dry, appliance/electronicsSS304
Automotive cabin & engine baySS304
Underbody, road salt, winter testingSS316
Coastal, marine, chemical washdownSS316
Deep draw with very thin walls (cost-sensitive)SS304, if environment allows

If you’re unsure where your application falls, send us the operating environment with your drawing — our team reviews material selection as part of every quote, at no charge.

Looking for examples? Browse our deep drawn sensor housing case study or the full range of sensor housings we manufacture.

What the standards actually specify

SS304 and SS316 are both austenitic stainless steels: the same face-centred-cubic grain structure, the same non-magnetic behaviour in the annealed condition, and the same inability to harden by heat treatment. What separates them is the alloy content, and molybdenum is the only addition that changes the corrosion conversation:

ElementSS304 (EN 1.4301)SS316 (EN 1.4401)
Carbon (max)0.07%0.07%
Chromium17.5–19.5%16.0–18.0%
Nickel8.0–10.5%10.0–14.0%
Molybdenum—2.0–3.0%

Everything a designer feels downstream — forming behaviour, springback, the surface after drawing — follows from that one column difference. It is also why the two grades run on the same tooling: the press, the dies and the lubricant are unchanged; only the incoming coil and its paperwork differ.

How we verify what arrives at the dock

Mixed lots are the failure mode nobody plans for. Every coil we draw arrives with a mill certificate to EN 10204 type 3.1 carrying its heat number, and that heat number stays with the lot through blanking, drawing and shipping — so a housing that comes back from the field two years later can still be traced to the melt it came from. For programmes where the grade is warranty-critical we also run positive material identification on incoming stock, because 304 and 316 are indistinguishable by eye once they are drawn and finished, and a mislabelled reel of 304 inside a 316 job is exactly the claim this article exists to prevent.

Magnetism: the question sensor customers forget to ask

Both grades are effectively non-magnetic in the annealed state, which is a large part of why they appear in sensor packages at all. Deep drawing is cold work, though, and cold work raises magnetic permeability slightly as the austenite begins to transform. For most housings the effect sits far below what a Hall-effect or reed sensor will notice. Where the sensing element sits millimetres from the shell wall — proximity packages, some current-sensing designs — we discuss the annealed condition and the deformation history during quoting, because at that distance the grade question stops being a materials question and becomes a layout question.

Lubricant chemistry is part of the corrosion decision

Chlorinated drawing lubricants are excellent at the press and troublesome afterwards: they leave chloride residues in the very recesses the drawing process creates. On a housing destined for a salt-spray environment, that residue is a pitting initiator waiting for the first winter. For harsh-duty sensor shells we run non-chlorinated lubricants, add a post-draw cleaning step before passivation, and record the surface condition on the inspection report. The grade sets the ceiling on corrosion performance; the process decides whether the part actually reaches it.

Finish options after drawing

Drawn stainless steel housings ship in two surface conditions for most programmes: as-drawn bright, or passivated to ASTM A967. As-drawn bright is the default — the drawing process leaves a clean, smooth surface that most sensor applications never touch afterwards. Passivation is specified where the housing will sit in a humid or chemical environment, because it removes the free iron the tooling leaves behind and lets the chromium oxide layer reform properly. Where a thicker barrier or a specific colour is needed, plating and coating run through qualified partners under our quality system, with the coating allowance on mating diameters designed into the tooling from the start rather than corrected afterwards.

Whichever grade wins, the deep drawing process covers how each behaves across stages, and the force and LDR calculator shows whether the difference is enough to change the stage count.

Frequently Asked Questions

Can you tell SS304 and SS316 apart just by looking at them?

No. Once drawn and finished, the two grades are visually identical. Identification needs positive material identification on the part, a spark test on the raw material, or the mill certificate — which is why we certify by heat number rather than by appearance.

Is SS316 worth the premium for indoor electronics?

Almost never. Indoor, dry environments never come close to challenging the chloride limit of 304, and 304 draws slightly better, so paying the 10–20% material premium usually buys a marginally looser part. SS316 earns its cost when road salt, marine air, cleaning chemicals or process fluids are part of the service environment.

Does passivation make SS304 corrosion-proof?

No. Passivation removes free iron embedded from tooling and rebuilds the chromium oxide layer, restoring the grade’s native resistance — but it does not add chloride resistance. A passivated 304 housing still pits in salt spray, which is why we treat passivation as standard practice, not as an upgrade to 316.

Will a drawn stainless steel housing interfere with a magnetic sensor?

Both grades are non-magnetic in the annealed condition, and drawing raises permeability only slightly. For sensors mounted close to the shell we discuss material condition and geometry at the quoting stage so the stack-up is settled before tooling is cut.

Do you supply material certificates?

Yes. We issue EN 10204 type 3.1 mill certificates with heat-number traceability, and the certificate stays attached to the lot through production so the paper trail and the parts never separate.

Can the grade be changed after tooling is cut?

In most cases yes, because the tooling is grade-independent: the forming behaviour of the two grades is close enough that the same dies run both. We confirm against your geometry before committing, since deep, thin-wall shells are where the work-hardening difference shows up first.

Does 316 stainless steel draw differently from 304?

Not much in the press. Both are austenitic, work-harden quickly and sit in the same draw-ratio band on our line (1.85–2.05 for 304). 316 adds 2–3% molybdenum for chloride resistance, which matters in service rather than in the draw. Both are supplied against ASTM A240/A240M; choose the grade for the environment and expect the certificate requirements to affect price more than the stage plan.

Related reading

Limiting Draw Ratio (LDR) Reference for Deep Drawn Parts — first-draw limits by material with stated test conditions, wall-thinning data and a blank diameter calculator.

References & Standards

The grade choices and formability notes on this page reflect the material properties these standards define. We verify each lot on incoming inspection rather than trust the mill certificate alone.

  • ASTM E646 — Standard Test Method for Tensile Strain-Hardening Exponents (n) of Metallic Sheet Materials. The n-value sets how much a wall can thin before necking.
  • ASTM E517 — Standard Test Method for Plastic Strain Ratio (r) of Sheet Metal. The r-value predicts earing in drawn cups.
  • DIN 8584 — Manufacturing processes, forming: classification of deep drawing operations and their subgroups.
  • Wikipedia: Sheet metal — material grades, gauge and formability background.
  • Wikipedia: Anisotropy — explains the r-value and why earing directions form.

Key point: Choose 304 stainless steel for general sensor housings and 316 stainless steel when chloride exposure calls for a molybdenum-bearing grade.

What we do not claim: We do not publish leak-rate figures, autoclave cycle counts or springback angles that we have not measured. The ±0.02 mm figure applies to ironing passes only, not to every geometry. 6xxx aluminium is used for shallow forming, not deep drawing. Prices, minimum order quantities and lead times are confirmed per drawing rather than published as fixed values.

Last reviewed: 2026-11-05 · Reviewed by Sam Zhang, Process Engineer