
Zinc plating is a spec with a thickness, and the thickness is a functional decision
“Zinc-plated steel stamped part” sounds like a commodity description, and on a purely cosmetic part it can be. But zinc plating on a stamped steel component is not a surface treatment – it is a sacrificial corrosion protection system with a design life, and it has three properties that have to be designed for: it grows on the part, it is soft, and it fails by consuming itself. A drawing that specifies “zinc plated” without stating a thickness class has specified a range rather than a requirement, and the range is wide enough that parts from two batches can behave very differently.
We die-stamp these with in-press forming and piercing, logging every stage against your part number, on 5-250 T mechanical presses with dedicated dies, secondary operations on CNC turning centres, and CMM inspection. Pierced holes are held to +/-0.03 mm and formed sections to +/-0.1 mm, with critical dimensions carrying CMM data with the shipment. SPCC and DC01 cold-rolled carbon steel in 0.5-3.0 mm is the standard stock, with pickled (SPHC) or galvanised alternatives. Made to your 2D or 3D drawings in PDF, DWG, STEP or IGS, samples are reverse-measured into a controlled drawing and the same drawing is used for every repeat order. This page is about the plating specification itself, and about what a stamped part needs from it.
Plating thickness classes, and why the class is the requirement
Electroplated zinc on steel is specified in thickness classes, and the classes exist because the service environments they suit consume zinc at very different rates. The logic is simple and worth understanding:
| Interior, dry, no exposure | Thin plating is sufficient. The zinc is present to prevent white rust during handling and storage, not for corrosion protection. |
|---|---|
| Enclosed but humid | Moderate plating. The environment is not wet enough to wash zinc off quickly, but there is enough moisture to consume thin coatings. |
| Exposed indoor | A heavier class, and the point where sacrificial protection genuinely starts to matter. |
| Outdoor, sheltered | Heavy plating, and the expectation that the part will be re-plated or replaced within a defined service life. |
| Outdoor, exposed or industrial or marine | The hardest case. Here zinc alone is often insufficient and a zinc-flake or a duplex system is the right answer – and this is the point at which “zinc plated” stops being the correct specification and should be changed on the drawing. |
Two of those entries are worth expanding. First, zinc is sacrificial: it corrodes preferentially to the steel, which is exactly what protects the steel. This means a zinc-plated part that has rusted a little is doing its job – but it also means the coating is consumed over time and the protection is finite. Second, the failure mode in a salt environment is white rust of the zinc, which appears early and looks catastrophic while the steel underneath is still perfectly sound. Distinguishing that from actual steel corrosion is a useful field diagnostic and it is one reason people over-specify.
Growth: the dimension problem is unavoidable
Electroplating grows on a sacrificial layer, so every plated surface moves outward. On this part’s stated tolerances this is not a rounding matter:
- Pierced holes at +/-0.03 mm become smaller by roughly twice the plating thickness. On a clearance hole this is harmless; on a locating hole or a dowel hole it is a fit change and must be specified as a post-plate dimension.
- A shaft that something slides over must be specified post-plate, or given a plating allowance. This is the classic failure: a part that is at nominal size before plating and 0.04 mm oversize after, and does not assemble.
- A flat face that seats against another part grows by the plating thickness, which tilts the joint slightly if only one surface is plated.
- A stamped part’s formed sections are typically specified at +/-0.1 mm, so plating is comfortably inside that band – which is why the plate-dimension question only bites on the features that are held tighter.
The correct practice is to state which dimensions apply before plating and which apply after. On a stamping with a mixture of features this is a normal part of the drawing rather than an exception, and getting it wrong is one of the more reliable ways to produce a batch that cannot be assembled.
Coverage: where plating is thinner than expected
On a stamped part there are specific locations where plating coverage is a real concern, and each has a remedy that belongs on the drawing:
- The inside of a pierced hole. Plating solution has to reach it and current has to flow there. Deep holes and holes with a poor entry angle are thinnest at their bottom and on the side walls, and a functional bore in a plated part should be masked.
- Sheared edges and burrs. A sheared edge is where the coating bridges from one face to another, and it is thinner than the flats, sometimes much thinner. A stamped part’s burr edges are the first place a plated coating fails.
- Formed radii and the inside of a bend. Better coverage than holes, but still measurably thinner than the flats because the throwing power of the solution is limited.
- Deep drawn cavities. A cavity’s interior is the worst-covered area on a stamped part. Where a cavity will hold water or is a corrosion-critical area, this needs to be a stated requirement and sometimes a design change.
- Threads. Almost always thinner than nominal and frequently specified outside the tolerance. Threads should be masked, and if a plated thread is genuinely wanted the plating class and the thread tolerance have to be agreed together.
Appearance and the question of what a part should look like
Natural, plated or coated – the print decides, the agreed finish is logged, and finish thickness and adhesion is checked on the first article. On a zinc-plated stamped part, appearance has three components and each is controllable separately:
- Colour and brightness. A bright passivated zinc, a matte zinc, a chromate-free passivate, and the coloured chromate conversion coatings each look different. On a visible part, the finish should be described by an agreed reference sample rather than by a name, because the same name covers a range of appearances.
- Spangle. A zinc deposit on a larger part can develop a crystalline pattern. On a formed stamping the pattern follows the form, and it is a normal characteristic rather than a defect – but if the part is visible, it should be agreed.
- Hydrogen embrittlement. This is the one to take seriously. Electroplating can hydrogen-embrittle a cold-worked steel, and a stamped part from 0.5-3.0 mm cold-rolled steel is work-hardened by the forming itself. On a load-bearing or safety-critical part, hydrogen embrittlement is a real failure mode with a serious consequence, and the mitigation is a baking step after plating with a defined delay. This should be specified, not assumed – particularly on a higher-strength or heavily formed part.
Material: SPCC, DC01, and the alternatives
SPCC and DC01 cold-rolled carbon steel in 0.5-3.0 mm is the standard stock for a formed component, with pickled (SPHC) or galvanised alternatives. The choice for a zinc-plated stamping:
- SPCC and DC01. The general grades. DC01 has tighter surface and mechanical property tolerances than SPCC in most relevant respects, and on a part with a demanding flatness or form requirement the higher-specified grade is usually the better choice.
- Higher-strength grades where the part needs to be strong at a given thickness – which also means hydrogen embrittlement becomes a serious consideration and a baking requirement becomes essential.
- Pickled (SPHC) stock where the surface condition matters – an appearance-critical part, or a part that will be coated rather than plated, where surface scale interferes.
- Galvanised (hot-dip) material as an alternative, and here the differences are significant enough to state: hot-dip galvanising gives a much thicker, harder, spangled and less uniform coating than electroplating, and it changes dimensions far more. A design that suits electroplated zinc frequently does not suit hot-dip without review, because the coating thickness alone can exceed a dimensional tolerance.
What to state on the drawing
Made to your 2D or 3D drawings in PDF, DWG, STEP or IGS, with samples reverse-measured into a controlled drawing and the agreed version governing every later batch. Die design and toolmaking stay in house, so no tooling step is outsourced, and first-article timing is measured from the tooling start date. Prototype and pre-production samples are provided against the drawing, the approved first article becomes the gauge reference, and the signed sample is kept for future reorders.
Eight things that make a zinc-plated stamped part right first time:
- The plating system and thickness class, named rather than left as “zinc plated”.
- Whether dimensions are before or after plating, feature by feature where it matters.
- Which features are masked, and specifically threads, locating bores and sealing faces.
- Whether hydrogen embrittlement is a concern, and if so a baking requirement with a defined delay.
- The passivate type, and where chromates are restricted, the compliant alternative.
- An appearance reference sample, if the part is visible.
- The service environment, so the plating class can be chosen rather than defaulted – and so a decision to move to a zinc-flake or duplex system can be raised if the environment is severe.
- The steel grade, confirmed in writing, since it drives both the formability of the stamping and the embrittlement question.
And the practical warning worth repeating: on a part specified at +/-0.03 mm on pierced holes, plating is not a finishing detail. It is a dimensional operation with a tolerance of its own, and specifying it properly is the difference between a part that assembles and a part that does not.
Custom Metal Stamping Parts is the range this part sits under; the overview page pulls together the tooling logic, finishing options and tolerance notes that apply across the family.
Specifications
| Item | Zinc-Plated Steel Stamped Pivot Bracket |
|---|---|
| Brand | AUNOV |
| Designing | Made to your 2D/3D drawings (PDF, DWG, STEP, IGS) – samples are reverse-measured into a controlled drawing; the agreed version governs every later batch. |
| Tooling | Die design and toolmaking stay in house, so no tooling step is outsourced, and first-article timing is measured from the tooling start date. |
| Samples | Prototype and pre-production samples are provided against the drawing, so the approved first article becomes the gauge reference, and the signed sample is kept for future reorders. |
| Materials | SPCC / DC01 cold-rolled carbon steel, 0.5-3.0 mm, the standard stock for formed component; pickled (SPHC) or galvanised alternatives. |
| Surface finish | The print decides between natural, plated or coated; we log the agreed finish and check thickness and adhesion on the first article. |
| Processing | Die stamping with in-press forming and piercing; every stage is logged against your part number. |
| Equipment | Press shop with 5-250 T mechanical presses and dedicated dies; secondary ops run on CNC turning centres, inspection on the CMM. |
| Tolerance | +/-0.03 mm on pierced holes, +/-0.1 mm on formed sections; critical dimensions carry CMM data with the shipment. |
| Delivery terms | Terms are FOB by default, with CIF and DDP quoted on request and freight priced to your door. |
Related Products
Request a Quote for This Part
Send a drawing or sketch — get material advice, tooling cost and a per-piece price within 24 hours (working days).




