Zinc Die-Cast Housing Components with Machined Bores

Zinc Die-Cast Housing Components with Machined Bores
Zinc Die-Cast Housing Components with Machined Bores

A machined plastic part is a strange thing to specify, because the material is not dimensionally stable in the way metal is. Nylon in particular absorbs moisture from the air, and as it does it changes size – not by microns, but by a fraction of a millimetre or more on a part of moderate size. A tolerance written on a nylon part is therefore a tolerance written at a specific humidity, and the number on the drawing says nothing unless the condition is stated.

That is the central fact about this part, and everything else – the material grades, the machining approach, the threads, the inserts – follows from it or from the fact that plastic has no useful thread strength.

Nylon’s moisture problem, and why it is not a minor effect

Nylon is a polyamide, and polyamides are hygroscopic. The absorbed water acts as a plasticiser and it also occupies space in the polymer’s amorphous regions, so the part both grows and changes properties. The effects compound:

  • Dimensional growth. The growth is largest across the flow direction and smallest along the fibres, which means a part machined from extruded bar grows differently depending on which way the machining exposed the material. On a simple cylindrical part from round bar, the growth is roughly isotropic and predictable. On a part cut from a plate with features in several directions, the growth is not.
  • Property changes. Absorbed moisture raises the ductility and lowers the modulus. A part that is stiff and crisp when dry becomes noticeably more flexible at 60 percent relative humidity. On a part that locates something by its stiffness, that is a functional change, not a dimensional one.
  • The size of the effect. For unfilled nylon the dimensional change over a wide humidity range is on the order of a percent. On a 60 mm long part that is over half a millimetre. That is several times a typical machined tolerance, on a part that measured perfectly when it left the machine.

So the practical discipline on a nylon part is: state the reference condition. Relative humidity and temperature at which the dimensions apply. A tolerance specified at 50 percent relative humidity and 20 degrees is a real, reproducible specification and it can be held. A tolerance specified at nothing is a tolerance that will be argued about.

And it is worth noting that the fix is available if the dimension has to be held across environments: glass-filled nylon has a much lower moisture take-up and a much lower dimensional change, at the cost of harder machining, more tool wear, and a different surface. Acetal is another good dimensional-stability choice. So “nylon” as a specification is under-determined and there are usually better answers available once the stability requirement is known.

Threads in plastic, which are the worst feature on the part

A plastic part’s thread is the feature most likely to fail in service and the one most often drawn as if it were a metal thread. The reality:

  1. A plastic thread has far less stripping strength than its own material suggests. Because the material’s strength scales with the amount of material engaged, and because plastic’s modulus is low, the failure is usually the first thread stripping rather than the root breaking. A 0.5 mm pitch plastic thread has several engaged turns and each is weak.
  2. The torque needed to break the plastic can be close to the torque needed to strip the fastener. There is no useful warning. This is why plastic threads are usually assembled with a fastener of a controlled grade and a controlled torque, or with a metal insert.
  3. Thread inserts solve most of it. A brass or stainless steel insert moulded or pressed into the plastic gives a metal thread with a normal strength and a normal torque. It costs an operation and it makes the hole a real feature to be specified – its position, its diameter, and whether it is moulded in or inserted after machining. On a part that will be assembled and disassembled more than a few times, the insert is normally the right answer.
  4. Where a plastic thread is genuinely right, it is where the fastener is plastic too, or where the joint is permanent, or where the torque is very low. In those cases the requirement is that the thread be long enough for the intended engagement and that the first engagement be a full-diameter lead rather than a partial thread, because starting a plastic thread part-way is how it gets stripped.

How plastic machines, and why the sequencing is different

CNC turning from bar or billet with concentricity held across operations, first articles verifying the whole flow. The route is right; the approach is not the same as metal.

  • Speeds are high and feeds are light. Plastic cuts far faster than steel, and the limiting factor is often the spindle power required to avoid rub rather than the cutting speed available.
  • Heat is the enemy, and it comes from the tool rubbing rather than from cutting. Plastic has a low thermal conductivity and a low melting point. A tool that rubs will smear the surface, and a smearing surface is not just cosmetic – it can hold the part in the chuck and it can cause the tool to pick up. Sharp positive-rake tooling and good chip evacuation are not preferences here.
  • Elastomers and some plastics cannot be turned at all at reasonable rates because they deform elastically. A part in such a material is usually ground or moulded rather than turned.
  • Reaming and tapping need chip control that metal does not. Plastic chips are long, sticky and gummy. They recut the surface and produce burrs. This dominates the achievable finish more than the tool’s condition does.
  • Deburring has to be thorough, because plastic burrs are sharp and will not break off. A plastic part that looks acceptable on the bench will have a burr that finds the assembly’s softest sealing face.

Material grades, and what each one changes

The route also lists carbon steel, 304 and 316 stainless steel, aluminium and brass alongside the plastics, which is worth separating out: on this page the metal grades are the alternative when the part turns out to need metal’s stability or its strength.

  • Unfilled nylon (PA6, PA66) – the strongest and the most moisture-sensitive. PA66 is dimensionally better than PA6 and is the general engineering choice.
  • Glass-filled nylon – far better dimensional stability, higher temperature resistance, harder to machine because of the abrasive glass, and it makes the surface look and feel different. On a part with any tight tolerance across a moisture cycle, this is the right answer.
  • Acetal (POM) – excellent dimensional stability, low friction, very machinable, and the right choice for a part with precise fits and low moisture exposure.
  • Polycarbonate – toughness and transparency, but it is stress-cracking-prone and it will crack around a sharp corner or a heavily threaded hole. If it is used, the corners need generous radii.
  • PTFE – almost nothing can be done to it conventionally. If PTFE appears on a machined-part enquiry, the realistic answer is moulded.
  • Composites and glass-reinforced thermoplastics – they machine but they change the whole approach, and the wear on the tooling is severe.

Design rules that make plastic parts work

The things that reliably separate a plastic part that works from one that fails are geometric, and none of them require a material change to achieve.

  • Radii everywhere. Sharp internal corners in plastic are stress concentrations and they are the initiation point for cracks. A 0.5 mm fillet in a corner costs nothing and prevents most of the failures. Plastic is the material where fillets matter most.
  • Wall thickness uniform. Varying wall thickness produces varying cooling and therefore varying internal stress and varying shrinkage. On a part with a nominal 2 mm wall and one spot at 4 mm, the 4 mm spot will have a different dimension.
  • No sharp changes of section near a fastener. A washer face on a thin wall will deflect and the fastener will not stay tight.
  • Avoid snap fits if the part will be assembled many times. A plastic snap fit wears in and its holding force drops over a few dozen cycles. If the joint must survive repeated assembly, a metal insert or a screw is the answer.
  • Think about what the part rubs against. A plastic bearing surface against a steel pin is fine; a plastic boss taking a steel fastener’s clamping directly is where failure starts.

Surface finish, marking and inspection

Natural, plated or coated per the print, with masking and laser marking available. On a plastic part the finish discussion is mostly about what should not be coated:

  • Plating a plastic part is metallisation, and it is a specialist operation – a conductive layer, then a plated layer. It is used for EMI shielding and for appearance. It is not a general coating option and it belongs on the drawing as a specific requirement with its own adhesion test.
  • Laser marking works well on plastics and is the right identification method, because it does not add thickness and it does not affect any fit.
  • Surface finish on a plastic functional face matters more than it looks. A tool-marked bore will have a higher friction coefficient against a pin than a polished one, and on a sliding plastic fit this shows up as wear.

Inspection on this part has one item that dominates the rest: dimensional inspection under a stated conditioning. Either condition the parts before measurement, or measure and report the humidity and temperature, or accept that a nylon part’s dimensions are only meaningful relative to a condition. On a first article that means conditioning to a defined reference before the CMM run. And it means the first article should be re-measured after a period in service conditions if the application involves a change of humidity, because that is the test that proves the material choice rather than the machining.

Beyond that: +/-0.01 mm on turned and milled features is achievable on rigid, filled plastics and is optimistic on unfilled nylon; burr condition on every edge, since burrs are not acceptable on plastic the way they sometimes are on metal; and thread condition on every thread, which on plastic means checking for a clean full-form thread and no partial-thread first engagement.

The humidity and temperature it will see in service

What humidity and temperature will this part see in service – and does it have to hold its dimensions across that range, or only at the moment it is assembled? If it only has to be right at assembly, unfilled nylon is cheap and easy and the tolerance can be written at the assembly condition. If it has to hold its position over a year through seasonal humidity changes, then the material choice is not a detail: it has to be a filled or low-hygroscopy grade, and the tolerance has to be written with a conditioning condition and the part has to be inspected after conditioning rather than off the machine. That second case is much less common than the first, and it is almost never raised at enquiry stage. Raising it there costs one sentence and it can change the material, the price and the lead time.

The CNC Machining Parts range is the parent for parts like this one; tooling logic, finishing options and tolerance notes for the whole family are gathered on its overview page.

Specifications

Frequently Asked Questions

Why is nylon’s moisture problem not minor?

Direct answer: Because nylon absorbs water, and as it does it swells and its dimensions and strength move. A nylon part that fits dry may bind or go out of tolerance in a humid environment. The moisture uptake is a real dimensional and mechanical effect, and it is designed for rather than ignored.

Why are threads in plastic the worst feature?

Direct answer: Because a thread concentrates stress in a material that is weak and creeps. A metal thread in a plastic part strips, and a self-tapping thread in plastic is a compromise. The thread is the feature most likely to fail, and it needs a coarse form and more engagement than a metal thread would.

Plastic heats and moves under the cut – how does that change the sequence?

Direct answer: Because plastic heats, softens and moves under the cut, so the sequence has to account for thermal growth and for the part’s flexibility. A plastic part is machined with lighter cuts and more support, and the finish comes from the tool’s geometry rather than from aggressive removal.

ItemZinc Die-Cast Housing Components with Machined Bores
BrandAUNOV
DesigningFiles reviewed in PDF, DWG, STEP or IGS; the signed-off revision is the reference for production.
ToolingProgressive and drawing dies are designed and built in house, so die cost stays transparent, and maintenance is tracked against the part number.
SamplesPre-production samples come with a full inspection report, so the approved first article becomes the gauge reference, and mass production is gated on that approval.
MaterialsStock covers carbon steel (SPCC / DC01), 304 / 316 stainless steel, aluminium and brass; grade and temper are confirmed in writing before tooling.
Surface finishNatural, plated or coated – the print decides, and the agreed finish is logged; masking and laser marking available where needed.
ProcessingCNC turning from bar or billet, concentricity held across operations; first articles verify the whole flow before the run is released.
EquipmentBar-fed CNC turning centres plus 3- and 4-axis machining centres, with CNC turning centres for secondary operations and CMM inspection.
Tolerance+/-0.01 mm on turned and milled features; dimensional reports accompany the first article.
Delivery termsCIF or DDP, with FOB available, T/T with deposit and L/C for larger runs; repeat orders reuse the approved first article.

Request a Quote for This Part

Send a drawing or sketch — get material advice, tooling cost and a per-piece price within 24 hours (working days).