A one-end-closed tube with a flange is a boundary, not a conduit. One end is a pressure boundary, the other is an interface to something else — a vessel, a manifold, a weldment. That distinction drives everything about the part, and it is the reason this component is specified so differently from a plain cut-and-deburred tube.
At 4mm outside diameter the whole part lives inside a wall thickness that is frequently under half a millimetre. Every forming and joining decision is made against that number, and the material grade decision — 316 rather than 304 — is a decision about where that thin wall will eventually be attacked.
Why 4mm is a harder diameter than it looks
A 4mm tube is small enough that the tolerance band on the wall competes with the tolerance on the diameter. This is not a philosophical problem; it is arithmetic.
- The outside diameter is measured directly with a micrometer and can be held to a tight band, because there is steel against air at that dimension.
- The wall thickness cannot be measured the same way at production rate. Every production method has an uncertainty — eddy current, ultrasonic and optical all carry an instrument band that is a meaningful fraction of a 0.3mm wall.
- The bore is the consequence. Bore equals outside diameter minus twice the wall, so the bore tolerance is twice the wall tolerance plus the diameter tolerance, and on a 4mm bore that can consume the entire allowable range.
What follows is a practical rule: on small-diameter tube, the outside diameter is the dimension to control tightly and the wall should be specified as a band with a stated measurement method. A drawing that quotes a single nominal wall with a tolerance and no method is a drawing that will produce disputes at incoming inspection.
316 does one specific job, and it costs you in two specific ways
304 and 316 differ mainly in molybdenum content — 316 carries roughly double. Molybdenum stabilises the passive chromium oxide film against chloride attack. That is the entire benefit, and it is a large benefit in the environments this part tends to see: coastal air, salt spray, washdown, process streams carrying trace chloride, and condensation that concentrates whatever salts are in the air.
The costs are worth stating plainly, because they are what makes 316 the wrong choice in some applications and the right one in others.
- Machining. 316 work-hardens faster and gouges more. It demands positive-rake geometry, sharp tools and no dwelling. A cutting tool that worked acceptably on 304 will produce a rough, torn surface on 316 and will work-harden the surface it cuts.
- Forming. Lower ductility at the same strength means a larger bend radius and a greater tendency to crack at the outside of the bend. The allowance for a formed feature on 316 should be larger than on 304.
- Welding. 316 is more prone to hot cracking if the restraint is high and the dilution uncontrolled. Welding consumables have to match or overmatch, and the heat input has to stay in a band.
Where the environment is dry and clean, 304 is the correct and cheaper answer. Where chloride exposure is real and continuous, 316 is the only version of this part that will survive. Specifying 316 as a default without an environmental basis simply raises the cost.
The closed end is the highest-risk feature on the part
Forming a closed end means creating a transition from a cylindrical wall to a flat or dished bottom. That transition is a stress concentration, and how it is made determines the whole part’s life.
There are three routes, in ascending order of quality:
- Flat end, formed by pressing. Fastest, cheapest, and the worst stress state. The bend from wall to floor is tight and the material is stretched hard on the outside of that bend. This is the classic configuration for a part that will eventually fail at the corner.
- Dished or radiused end. A formed radius between wall and floor. This is materially better because the strain is distributed over an arc instead of a sharp bend. The radius should be specified and it should be at least on the order of the wall thickness for a formed feature in 316.
- Full hemisphere. Formed hemispherical end on the tube. This is what a pressure vessel end cap is, and it is the only one of the three where the stress in the end is comparable to the stress in the wall.
Whatever the route, the material condition at the formed end is work-hardened and residual-stressed. If the end is later machined flat, the cut removes the material that was in compression on the outside of the bend and leaves the tensile zone exposed. This is why a formed-and-then-faced end needs a stress-relief anneal, and why that anneal should be specified rather than assumed.
A flange on a 4mm tube is a geometric decision, not a decoration
The flange serves three functions at once, and the drawing has to resolve all three.
Bolting. If the flange is drilled and bolted, the bolt circle, the bolt size and the flange thickness determine the seating face geometry. A flange that is thin relative to the bolt load will deform at the bolt holes and lose its flatness — the same failure mode as the poor flare seat described elsewhere in this family of parts.
Alignment. A flange face has to be flat within a parallelism band referenced to the tube axis. The tube axis is established by the drawn section; the flange is machined from it. If the flange is a separate welded piece, the weld introduces an error that the machining has to absorb.
Welding to the mating part. If the flange is meant to be welded rather than bolted, its edge preparation matters: bevel angle, root face, root gap. A square-cut flange cannot be welded reliably and will produce the porosity that a square-edge joint always produces.
The most robust construction for this part is an integral flange machined from solid or from a thicker section, with the tube body drawn and the end formed. That gives a single piece of material with no second joint to fail, and it lets the flange thickness be whatever the bolting needs while the wall stays as specified. It costs more in material and in machining time, and it is the version that goes into service.
Surface treatment has to be compatible with the service
Passivation is the default for stainless steel, and it is not decorative. The drawn and annealed surface carries free-iron contamination from the drawing dies and the tooling, and that contamination rusts. Passivation removes the free iron and restores the passive film.
Where a coating is applied instead, the following matters:
- Plating on a formed thin wall introduces hydrogen embrittlement risk unless a baking relief is specified.
- Electroless nickel is tolerant of complex geometry and coats uniformly, but its thickness on a thin wall is a meaningful fraction of the wall and its dimensional effect has to be accounted for at the mating face.
- Any coating on the sealing face changes the sealing behaviour. A gasket or a weld that was designed for a bare surface cannot be assumed to work on a plated one.
The sealing faces are the exception, not the default. Whatever coating is specified, the faces that seal should be called out as masked or as bare.
Inspection that actually discriminates
- Diameter and wall. Wall by a stated method with the instrument uncertainty declared; diameter by micrometer at multiple positions to detect ovality.
- Formed end geometry. The end-to-wall transition radius measured, and the end depth measured from the tube axis reference. This is the dimension that identifies whether the correct forming route was used.
- Flange flatness and parallelism. Over the full face, referenced to the tube axis. Not just thickness.
- Bore and concentricity. The bore is small on a 4mm part, and its inspection catches the drawing-die condition that a diameter check would miss.
- Pressure or leak test. On the finished part, at design pressure, with the pressure-holding time and the pass criterion stated.
- Surface condition on the formed end. Visual plus dimensional, to confirm the anneal and finishing did not leave surface breaking or excessive roughness that would be a crack initiation site.
Questions worth asking before releasing the drawing
- Is the wall specified as a band with a stated measurement method, and is the resulting bore tolerance actually acceptable downstream?
- Is the environmental basis for 316 documented — chloride concentration, exposure type, duration — or is the grade inherited by habit?
- Is the transition between wall and closed end radiused, and is that radius dimensioned rather than being whatever the tool produces?
- Is the flange integral to the part, and if so is its thickness driven by the bolting load and the required flatness?
- If the closed end is machined after forming, is a stress-relief anneal specified between the two operations?
- Are the sealing faces excluded from any coating, and is that exclusion on the drawing?
- Does the part get a pressure or leak test at final inspection, or is it accepted on dimensions alone?
That last question is the one that separates a part that can be delivered from a part that can be used. A thin-wall closed tube that passes every dimensional check can still be a leaking part if the closed end carried a through-crack from forming and nothing in the inspection plan can detect it. Only a pressure test detects it, and on this geometry it is cheap.
Deep Drawn Tubes & Sleeves is the parent range for parts like this one; the overview page gathers the tooling logic, finishing options and tolerance notes that apply across the family.
Where this part is used
A one-end-closed tube with a flange at 4 mm outside diameter lives in a world where the tolerance on the wall competes with the tolerance on the diameter. That is not a philosophical problem, it is arithmetic: the bore equals the outside diameter minus twice the wall, so a small wall band consumes a large share of the available bore tolerance. These parts turn up in capillary assemblies, in small-bore fluid fittings, in instrumentation where a sealed port and a mounting face are needed on the same component, and in miniature sensor bodies.
The flange makes it a boundary rather than a conduit. One end carries pressure or a fluid, the other mates to something – a manifold, a vessel, a clamp – and that second duty is why the flange’s geometry is designed rather than added. On a 4 mm tube a flange is a small formed or machined feature whose flatness and bore concentricity have to hold against a wall that is often under half a millimetre.
What we need to quote it
Send the outside diameter, the wall band you need and the measurement method you will use to verify it – eddy current, ultrasonic or optical – because a single nominal wall with a tolerance and no method is a drawing that produces disputes at incoming inspection. Tell us what the closed end has to hold, what the flange mates to, and the service environment so the grade and the surface treatment can be matched. If you have a sample, a measurement report on it settles the wall question faster than a drawing.
Specifications
| Item | Custom 316 grade OD 4mm stainless steel one end closed tube with flange |
|---|---|
| Brand | AUNOV |
| Designing | Your drawing sets the part – samples are reverse-measured into a controlled drawing; changes are priced before they are made. |
| Tooling | Our toolroom covers die design, wire-cut EDM and maintenance, so the die charge appears as its own quotation line, and the die remains dedicated to your part. |
| Samples | Samples are issued for approval before the run, and production starts only after written sign-off. |
| Materials | 304 / 316L stainless steel in 4 mm sheet for drawn and formed features, or bar stock for machined ones; mill certificate per heat on request. |
| Surface finish | Zinc, nickel or chrome plating, anodising, passivation or e-coat; masking and laser marking available where needed. |
| Processing | Precision tube drawing, cut to length and turned to the print; in-process checks sit between stages, not only at the end. |
| Equipment | Tube drawing lines with annealing and finish-turning cells, with in-house toolmaking to keep dies and fixtures maintained. |
| Tolerance | +/-0.05 mm on bore, wall thickness band confirmed at first article; finer bands confirmed from capability data before quoting. |
| Delivery terms | FOB, CIF or DDP per Incoterms 2020, T/T or L/C, with D/P accepted on repeat business; each volume tier carries its own quoted price. |
Related Products
Request a Quote for This Part
Send a drawing or sketch — get material advice, tooling cost and a per-piece price within 24 hours (working days).