A capillary tube is the least impressive-looking component in a refrigeration circuit. It is a length of small-diameter metal with no moving parts, no seats, no electronics. It is also the part that decides whether the system moves the amount of refrigerant the drawing promised, and whether it still does so after ten years of cycling.

That responsibility sits on a dimension nobody looks at. The outside diameter is checked with a micrometer and it is the dimension on the drawing that gets quoted. The bore is what actually meters flow, and the bore is set by the wall between it and the outside. Take the wall away and you have changed the capacity of the whole circuit.

The bore is a flow orifice, not a clearance

Refrigerant flow through a capillary is choked flow. Below the critical pressure ratio the tube behaves as an orifice with a predictable mass flow; above it, the flow becomes dependent on downstream conditions and the tube no longer behaves as a fixed restriction. Engineers therefore size the capillary from its internal length and internal diameter using a standard flow chart, then adjust for the inlet conditions of the specific refrigerant.

Two consequences follow, and both are frequently misunderstood.

  • The sizing calculation uses the internal diameter. Quoting a capillary by its outside diameter and a wall thickness tolerance band means the delivered part may fall outside the flow band even when every dimension on the print is satisfied.
  • Longer is not slower. Capacity falls steeply with length, so a capillary cut 5% long is a different component, not a slightly different component. Length control is a cutting operation, not a drawing operation.

Because the whole calculation collapses if the bore moves, the practical tolerance on the capillary bore is the tightest tolerance in the assembly, frequently tighter than the tolerance on any machined part in the same product. Where a print allows a generous band on the OD, that generosity is an economy in the material cost of the tube, not an engineering concession.

Wall thickness is a pressure class and a manufacturing record

The wall does three jobs at once. It carries the internal pressure, it carries the external handling loads, and it conducts heat from the refrigerant outward. In a capillary that last part matters less than people expect, because the refrigerant flow is already choked and the tube’s job is to resist heat gain rather than conduct it away.

Which is why stainless steel behaves so differently here from copper. Copper capillary tubes are common because copper is easy to draw to a thin, even wall and easy to braze. Stainless steel is used where the circuit sees corrosive service, where the tube runs through a salt-laden or food-processing environment, or where the specified refrigerant and lubricant combination attacks copper.

In return, stainless steel gives up a large factor of thermal conductivity. For a capillary whose capacity is deliberately set by geometry, that is often a benefit: a low-conductivity wall insulates the metering section from ambient heat, so the flow is less sensitive to the room temperature it happens to pass through. The same property that makes stainless steel difficult to braze becomes useful again once the part is finished.

Stainless Steel is also galled. When a stainless steel capillary is expanded into a flared seat, or when it is brazed into a fitting, the two stainless steel surfaces in contact can cold-weld. A thin film of nickel plating on the seating face, or the use of a dissimilar mating material at the joint, is standard practice and is worth specifying explicitly on the drawing.

Annealing is what makes the bore survive the draw

A capillary tube is drawn from a larger tube, usually several times. Each pass through the die reduces the diameter and the wall together. The material work-hardens; by the time the tube reaches its final size it is in a hardened, residual-stress state that is dimensionally accurate and mechanically unpleasant.

Two properties follow, and they pull in opposite directions.

  • Dimensional retention. A hardened tube holds its size. For a metering element this is valuable, and it is the reason drawn capillary is preferred over a tube that is merely cut to length.
  • Formability. A hardened tube resists flaring, bending and expansion. If the capillary end has to be flared for a flare nut connection, it must be annealed first, or the flare will crack along the length of the bore rather than form a clean cone.

Annealing is done in-line during drawing, between passes, on equipment sized so that the tube is never fully cold-worked through to the final pass. Annealed stainless steel capillary is softer, more formable and slightly less dimensionally stable, so the temper condition has to be agreed for the geometry in hand: hardened where the tube is only cut and crimped, annealed where it is flared or bent.

The end condition is where most capillary failures start

A capillary tube rarely fails in the middle. It fails at an end, and the two dominant end failures are both consequences of the wall thickness.

The first is a split at the flare. When the tube is expanded, the inner surface is stretched hardest. If the anneal was insufficient or the expansion was aggressive, the tube opens along the bore. This is visible as a leak at the flare, not at the tube, and it is easily misdiagnosed as a bad fitting.

The second is a cut end that is not actually square. A capillary tube is cut to length and then usually end-formed: flattened for a brazed capillary tube fitting, or flared. If the cut face is not perpendicular, the subsequent flattening produces a tube wall that is uneven along the circumference, and the thinned side tears under the expansion load.

The countermeasure is not a better operator. It is to make the end condition a controlled geometry on the drawing: specify the cut length, the perpendicularity of the cut, the flattened thickness and its direction, and the flare angle. Then the end operation can be verified with a go/no-go gauge rather than judged by eye. Every capillary tube that is going to be flared should have its flare gauged, because the gauge is cheaper than the return.

Stainless Steel grades and the ones that are actually different

Not every stainless steel capillary is 304. The grades differ in exactly the way that matters for a thin-wall pressure part: chloride resistance and weldability.

  • 304 / 304L. The general grade. Fine in dry service; will pit in chloride-bearing environments and is prone to stress-corrosion cracking in the presence of chlorides and residual tensile stress. The low-carbon variant is preferred where the capillary will be welded.
  • 316 / 316L. Roughly double the molybdenum content of 304. This is the grade that survives sea air, salt spray and many process chemicals, and it is the default for a capillary used outdoors or in a washdown environment.
  • Welded grade. If the capillary carries high pressure or feeds a hermetic system, specify the welded grade. A longitudinally welded capillary has a seam, and the seam is the only place on the tube where the material is not continuous.

The grade decision propagates into the process. A 316 capillary is harder to draw than a 304 one, so it narrows the workable wall band; it needs a more aggressive anneal schedule to recover formability for flaring; and it will not tolerate a ferritic or brass seating nut without a plating barrier to prevent galvanic corrosion.

Questions worth asking on the drawing

A capillary tube is easy to specify badly because none of the critical dimensions are the ones people look at. These are the questions that change the part:

  • Is the flow size quoted against the internal bore with a tolerance, or against the outside diameter with a wall band? If the second, the part cannot be verified as a metering element.
  • What is the specified temper — hardened or annealed — and does the end forming agree with that choice?
  • Is the cut length controlled, and is perpendicularity of the cut face an inspection point rather than an assumption?
  • If the tube is flared, what seating material is specified against the stainless steel to prevent galling and galvanic attack?
  • For a welded capillary, which grade is called out, and where along the length is the seam oriented relative to the flare?

The last question is the one most often left open. A welded capillary is a perfectly good component, but its seam has a preferred orientation for forming. If the part is flared afterwards and the seam happens to lie in the flare plane, the flare will open along it every time. Specifying the seam orientation costs nothing at quotation time and removes a whole class of returns.

This part belongs to our Deep Drawn Tubes & Sleeves range. The deep drawn tubes & sleeves pages collect the process notes, common materials and inspection points behind every product in the family.

Specifications

Frequently Asked Questions

Is a capillary bore a clearance or a flow orifice?

Direct answer: On a capillary it is a flow orifice. The bore is not there to let something slide through it; it meters flow, so its size and its roundness are a flow-control requirement. A bore that is the right size but slightly oval changes the flow for a given pressure drop, which is why on a capillary the bore is treated as the part’s functional feature rather than a clearance.

Where do most capillary failures start?

Direct answer: At the end condition. The cut end, the burr and the chamfer are where a capillary is most likely to leak, to scratch a mating seal, or to trap contamination. The end is the part’s interface, and a clean, burr-free, properly conditioned end is what separates a capillary that works from one that fails at the joint.

The bore survives the draw because of one scheduled step – which one?

Direct answer: Because annealing is what lets the bore survive the draw. A stainless steel capillary work-hardens as it is reduced, and without an anneal at the right point the next draw tears or leaves the bore stressed. The anneal is scheduled into the route card so the final bore is round and stable rather than a surface that will move later.

ItemStainless Steel Capillary Tube
BrandAUNOV
DesigningQuotation follows the print, not a catalogue – DFM notes are returned before any tooling is cut; revisions are re-quoted once rather than silently absorbed.
ToolingTooling is built and held under your part number, so no tooling step is outsourced, and first-article timing is measured from the tooling start date.
SamplesPre-production samples come with a full inspection report, so any deviation is corrected at sample stage, and later batches are gauged back to the signed sample.
MaterialsStandard stock: carbon steel (SPCC / DC01), 304 / 316 stainless steel, aluminium, brass; special grades are sourced to the drawing when volumes justify.
Surface finishNatural, plated or coated – the print decides, and the agreed finish is logged; masking and laser marking available where needed.
ProcessingTube drawing with precision turning on critical diameters; first articles verify the whole flow before the run is released.
EquipmentDrawing benches, annealing furnaces and CNC turning for tube ends, backed by CNC turning centres and a climate-controlled inspection room.
Tolerance+/-0.03 mm on machined ends, straightness per print; critical dimensions carry CMM data with the shipment.
Delivery termsFOB, CIF or DDP per Incoterms 2020, payment by T/T or L/C, quoted in USD or EUR; sea or air freight is quoted to your door.

Request a Quote for This Part

Send a drawing or sketch — get material advice, tooling cost and a per-piece price within 24 hours (working days).